 Medway Galvanising Co. Ltd Castle Road Eurolink Industrial Centre Sittingbourne Kent ME10 3RN Telephone : 01795 479489 Fax: 01795 477598
E-mail: medgalv@medgalv.co.uk Website: www.medgalv.co.uk
|
Bath Size 6.7m x 1.34m x 2.40m 3.66m x 1.2m x 0.79m Double Dip 12.0m x 1.3m x 0.6m or 6.7m x 1.34m x 4.8m
other sizes on application Maximum Lift 3.2 tonnes 0.5 tonnes Main Classes of Work General Centrifuged
Additional Facilities and Services Registered to BS EN ISO 9002 Centrifuge for spin galvanizing Powder coating after galvanizing with guarantees of up to 25 years Grit blasting Pickling Thread brushing T-wash
|