Galvanizers in  Wales

Cardiff Galvanizers (1969) Limited

Cardiff Galvanizers (1969) Limited

Address:
Cambria House
East Moors Road
Cardiff
CF24 5EG

Telephone:02920 480321
Fax:02920 483728
Email: info@cardiffgalvanizers.co.uk
Website: http://www.cardiffgalvanizers.co.uk/

Bath size:
7.0m x 1.5m x 3.0m

Double dip:
up to lengths of 12.5 m long and frames 4.5 m x 6.5 m

Max lift:6 tonnes

Main classes of work:
Centrifuged
Wirework
Sheet metals
Tanks
Castings
General

Additional features and services:
Registered to BS EN ISO 9002
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing
Sinking gear for hollow fabrications to be galvanized on the outside only
Thread brushing
T-wash

Ifor Williams Trailers

Ifor Williams Trailers

Address:
Cynwyd
Corwen
Denbighshire
LL21 0LS

Telephone:01490 412626
Fax:01490 412770
Email: sales@iwt.co.uk
Website: http://www.iwt.co.uk/

Bath size:
6.0m x 1.37m x 2.75m

Double dip:
Not applicable

Max lift:Not applicable

Main classes of work:
Own products

Additional features and services:
Registered to BS EN ISO 9002

Joseph Ash Galvanizing - Bridgend

Joseph Ash Galvanizing - Bridgend

Address:
Princes Way
Bridgend Industrial Estate
Bridgend,
Mid Glamorgan
CF31 3AQ

Telephone:01656 668735
Fax:01656 767139
Email: bridgend@josephash.co.uk
Website: http://www.josephash.co.uk/location/?/Bridgend

Bath size:
4.6m x 1.5m x 2.1m

Double dip:
Sizes on application

Max lift:4 tonnes

Main classes of work:
Fencing
Fabrications
Castings
Centrifuged

Additional features and services:
Registered to BS EN ISO 9002
ROSPA Gold Award 2016

Newport Galvanizers Limited

Newport Galvanizers Limited

Address:
Llanwern Works
Newport
Gwent
NP19 4QX

Telephone:01633 277400
Email: newport@wggltd.co.uk
Website: http://www.wedge-galv.co.uk/

Bath size:
6.8m x 1.1m x 3.5m

Double dip:
Sizes on application

Max lift:10 tonnes

Main classes of work:
Structural
Tubular
General

Additional features and services:
Registered to BS EN ISO 9001:2015
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing