Required fields

Clydeside Galvanizers Limited

Expressway Works
Eastvale Place
Glasgow
G3 8QG

Telephone: 0141 334 9678
Fax: 0141 337 1830

E-mail: ross@clydegalv.co.uk
Website: www.clydegalv.co.uk


Bath Size
7.0m x 1.3m x 2.0m

Double Dip
10.3m x 1.3m x 0.3m or
7.0m x 1.3m x 3.5m

 

 

 

 

Maximum Lift

5 tonnes

Main Classes of Work

Structural
Tubular
General
Tanks
Fencing
Offshore/Marine


Additional Facilities and Services
Registered to BS EN ISO 9002
Grit blasting
Pickling

Forfar Galvanisers Ltd

Carseview Road
Forfar
Angus
DD8 3BT

Telephone: 01307 460 222
Fax: 01307 460 444

E-mail: enquiries@forfar-galvanisers.co.uk
Website: www.forfargalvanisers.co.uk

Bath Size
5.5m x 1.4m x 2.8m

Double Dip
Not available

 

Maximum Lift

1.5 tonnes

Main Classes of Work
Structural
Pallets
Tubular
Gates
Fencing
Agricultural
General

Additional Services and Facilities:
Transport available
Shotblasting
Pickling
Registered to BS EN ISO 9001

Highland Colour Coaters 

 

Tower Road
Blairlinn Industrial Estate
Cumbernauld
G67 2JH

Telephone: 01236 731444
Fax: 01236 731555

E-mail: enquiries@higalv.co.uk
Website: www.higalv.co.uk


Bath Size
7.0m x 1.15m x 3.0m

Double Dip
Sizes on application

 

 

Maximum Lift
4 tonnes (powder coating 750kg per item)

Main Classes of Work
All general galvanizing undertaken

Additional Facilities and Services
Powder Coating
Centrifuge for spin galvanizing
Fusion Bonded Epoxy
Shot blasting
Transport Service

Registered to BS EN ISO 9001

 

Highland Galvanizers

 

Pinefield Industrial Estate
Elgin
Moray
IV30 6FG

Telephone: 01343 548855
Fax: 01343 545551

E-mail: enquiries@higalv.co.uk
Website: www.higalv.co.uk

Bath Size
10.5m x 1.05m x 2.5m

Double Dip
to 15m long, call for specifics
 

 

 

Maximum Lift
4 tonnes

Main Classes of Work
All general galvanizing undertaken

Additional Facilities and Services
Centrifuge for spin galvanizing
Shot Blasting
Transport service

Registered to BS EN ISO 9001

 

Scottish Galvanizers Limited

 

Maclellan Street
Glasgow
G41 1RR

Telephone: 0141 427 3041
Fax: 0141 427 4981

E-mail: scottish@wedge-galv.co.uk
Website: www.wedge-galv.co.uk

Bath Size
14.5m x 1.2m x 3.3m

Double Dip
24.0m x 1.1m x 0.5m
or
14.2m x 1.1m x 4.0m

 

 

 

Maximum Lift
10 tonnes

Main Classes of Work
Structural
Tanks
Castings
Tubular
General
Centrifuged

Additional Facilities and Services
Awarded "Investor in People"
Registered to BS EN ISO 9002
Centrifuge for spin galvanizing
Grit blasting
Transport service