Required fields


Galco Steel Limited

Galco House
Ballymount Road
Walkinstown
Dublin 12

Telephone : (01) 4506671
Fax: (01) 4566213

E-mail: info@galcosteel.ie
Website: www.galcosteel.ie


Bath Size
10.0m x 1.8m x 3.25m
4m x1.8m x 2.65m


Double Dip
16.0m x 1.6m x 0.5m
or
14.0mx 1.2m x 0.6m
by arrangement
9.0m x 1.2m x 4.0m

Maximum Lift
6.5 tonnes


Main Classes of Work
Castings
Centrifuged
Fabrications
Fencing
General
Pipes
Radiators
Structural
Tanks

Additional Facilities and Services
Grit blasting
Transport
Registered to IS EN ISO 9002

Galco (Cork) Limited

Tramore Road
Cork

Telephone: (021) 4312411
Fax: (021) 4312478

E-mail: info@galco-cork.ie
Website: www.galco-cork.ie


Bath Size
6.5m x 1.5m x 2.65m

Double Dip
By arrangement

Maximum Lift
5 tonnes

Main Classes of Work
Structural
Tanks
Pipes
Radiators
Castings
GeneralFencing

Additional Facilities and Services
Transport
Grit blasting

Galco (Waterford) Limited


Gracedieu Road
Waterford
Ireland

Telephone: (051) 874 254
Fax: (051) 874 456

E-mail: cpower@galcowaterford.ie
Website: www.galcosteel.ie


Bath Size
4m x 1.25m x 2.5m

Double Dip
Sizes on application

Maximum Lift
2 tonnes

Main Classes of Work
Structural
Tanks
Castings
General
Radiators
Fencing
Architectural
Agricultural
Designer commissions

Irish Pioneer Works (Fabricators) Limited


Kinsale Road
Cork

Telephone : (0214) 964299
Fax: (0214) 964110


Bath Size
7.5m x 1.0m x 2.0m

Double Dip
Sizes on application

Maximum Lift
3.2 tonnes

Main Classes of Work
Structural
Agricultural
General fabrications
Additional Facilities and Services
Centrifuge for spin galvanizing

Shannonside Galvanizing

4 Elms
Drombanna
Co. Limerick
Ireland

GPS: N 52 ° 37.20 W 08 ° 34.39

Telephone: (061) 412357
Fax: (061) 415853

E-mail: info@shannonsidegalv.com
Website: www.shannonsidegalv.com


Bath Size
12m long x 2m wide x 3.2m deep

Double Dip
22m long x 1.93m wide x 0.5m deep by appointment

Maximum Lift
6.4 tonnes

Main Classes of Work
Agricultural
Architectural
Castings
Designer commissions
Fabrications
Fencing
Gates
General
Pipes
Street Furniture
Structural
Tanks
Tubular

Additional Facilities and Services
Registered to BS EN ISO 1461 : 1999
Box profile cladding cut to size
Door track and fittings
Fabrication
Painting
Purlins cut to size
Steel stockists
Transport Service

Sperrin Galvanisers (Irl) Limited -me


Derryfrench
Tynegh
Laugh Rea
Co Galway
Ireland

Telephone: 00 353 90 9745 804
Fax: 00 353 90 9745 805

E-mail: tynagh@sperringalvanisers.com
Website: www.sperringalvanisers.com


Bath Size
7.0m x 1.4m x 3.2m

Double Dip
Sizes on application

Maximum Lift
5 tonnes
Main Classes of Work
Structural
Agricultural
Domestic