Clydeside Galvanizers Limited
Expressway Works
Eastvale Place
Glasgow
G3 8QG
Telephone: 0141 334 9678
Fax: 0141 337 1830
E-mail: ross@clydegalv.co.uk
Website: www.clydegalv.co.uk
Bath Size
7.0m x 1.3m x 2.0m
Double Dip
10.3m x 1.3m x 0.3m or
7.0m x 1.3m x 3.5m
Maximum Lift
5 tonnes
Main Classes of Work
Structural
Tubular
General
Tanks
Fencing
Offshore/Marine
Additional Facilities and Services
Registered to BS EN ISO 9002
Grit blasting
Pickling
Forfar Galvanisers Ltd
Carseview Road
Forfar
Angus
DD8 3BT
Telephone: 01307 460 222
Fax: 01307 460 444
E-mail: eoin.clarke@forfar-galvanisers.co.uk
Bath Size
5.5m x 1.4m x 2.8m
Double Dip
Not available
Maximum Lift
1.5 tonnes
Main Classes of Work
Structural
Pallets
Tubular
Gates
Fencing
Agricultural
General
Additional Services and Facilities:
Transport available
Shotblasting
Pickling

Highland Colour Coaters Ltd
Tower Road
Blairlinn Industrial Estate
Cumbernauld
G67 2JH
Telephone: 01236 731444
Fax: 01236 731555
E-mail: enquiries@higalv.co.uk
Website: www.higalv.co.uk
Bath Size
7.0m x 1.2m x 3.2m
Double Dip
Sizes on application
Maximum Lift
4 tonnes
Main Classes of Work
Agricultural
Tubular
Fencing
General
Additional Facilities and Services
Powder Coating
Centrifuge for spin-galvanizing
Electroplating
Shot blasting
Transport Service

Highland Galvanizers
Pinefield Industrial Estate
Elgin
Moray
IV30 6FG
Telephone: 01343 548855
Fax: 01343 545551
E-mail: enquiries@higalv.co.uk
Website: www.higalv.co.uk
Bath Size
10.5m x 1.1m x 2.5m
Double Dip
14.0m x 1.0m x 0.3m
or
10.0m x 1.0m x 3.4m
Maximum Lift
4 tonnes
Main Classes of Work
Agricultural
Offshore/Marine
Structural
Tubular
Fencing
Centrifuged
General
Additional Facilities and Services
Registered to
BS EN ISO 9002
Centrifuge for spin galvanizing
Electroplating
Fabrication
Grit blasting
Painting after galvanizing
Thread brushing
Transport service

Scottish Galvanizers Limited
Maclellan Street
Glasgow
G41 1RR
Telephone: 0141 427 3041
Fax: 0141 427 4981
E-mail: scottish@wedge-galv.co.uk
Website: www.wedge-galv.co.uk
Bath Size
14.5m x 1.2m x 3.3m
Double Dip
24.0m x 1.1m x 0.5m
or
14.2m x 1.1m x 4.0m
Maximum Lift
10 tonnes
Main Classes of Work
Structural
Tanks
Castings
Tubular
General
Centrifuged
Additional Facilities and Services
Awarded "Investor in People"
Registered to BS EN ISO 9002
Centrifuge for spin galvanizing
Grit blasting
Transport service