Cardiff Galvanizers (1969) Limited

Cambria House
East Moors Road
Cardiff
CF24 5EG

Telephone: 02920 480321
Fax:02920 483728

E-mail: sales@cardiffgalvanizers.co.uk


Bath Size
7.0m x 1.5m x 3.0m

Double Dip
9.0m x 1.1m x 0.3m
or
4.6m x 1.5m x 3.4m

Maximum Lift
4 tonnes

Main Classes of Work
Centrifuged
Wirework
Sheet metals
Tanks
Castings
General

Additional Facilities and Services
Registered to BS EN ISO 9002
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing
Sinking gear for hollow fabrications to be galvanized on the outside only
Thread brushing
T-wash

Ifor Williams Trailers

Cynwyd
Corwen
Denbighshire
LL21 0LS

Telephone: 01490 412626
Fax: 01490 412770

E-mail: sales@iwt.co.uk
Website: www.iwt.co.uk


Bath Size
6.0m x 1.37m x 2.75m

Double Dip
Not applicable

Maximum Lift
Not applicable

Main Classes of Work
Own products

Additional Facilities and Services
Registered to BS EN ISO 9002

Joseph Ash Galvanizers

Prince's Way
Bridgend Industrial Estate
Bridgend
Mid Glamorgan
CF31 3AQ

Telephone: 01656 668735
Fax: 01656 767139

E-mail: bridge@josephash.co.uk
Website: www.josephash.co.uk


Bath Size
4.6m x 1.5m x 2.1m

Double Dip
Sizes on application

Maximum Lift
4 tonnes

Main Classes of Work
Fencing
Fabrications
Castings
Centrifuged

Additional Facilities and Services
Registered to BS EN ISO 9002

Newport Galvanizers Limited

Llanwern Works
Newport
South Wales
NP19 4QX

Telephone: 01633 277400
Fax: 01633 277997

E-mail: newport@wedge-galv.co.uk
Website: www.wedge-galv.co.uk


Bath Size
7.0m x 1.22m x 3.73m

Double Dip
Sizes on application

Maximum Lift
6 tonnes

Main Classes of Work
Structural
Tubular
General

Additional Facilities and Services
Awarded "Investor in People"
Registered to BS EN ISO 9002
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing