Hot Dip Galvanizing

Proven, honest, sustainable

Galvanizers Association is the source of free information and advice about hot dip galvanizing, cost effective corrosion protection and the galvanizing industry. Feel free to contact us on +44 (0) 121 355 8838 if you need any assistance on design, specification or advice on performance.

Industry Open Day 2019 Square Banner 1

Industry Open Day

Free RIBA Approved Plant Tour

Various sites ranging from Elgin, Exeter, Hull and Galway in Ireland, will be opening their doors on October 15th.

The coordinated site visits are aimed at giving construction industry professionals a valuable opportunity to learn how to extend and improve their use of galvanizing.

Read about it

Rust Timelapse

the zinc tank

The Thing About Rust

Have you ever wondered what is going on with rusty steelwork? Why it happens and even what it is exactly?

Read more

 

Subscribe to the get the latest tech update via email
We launched ‘the zinc tank’, where we’ll inform you about the latest technical insights into the process, performance and the many uses of galvanized steel.

Featured Project
Imperial War Museum Studio Libeskind

Imperial War Museum

Studio Libeskind

The building is a simple interlocking of three shards, represent­ing Earth, Air and Water, constituting the various functions of the Museum.

The entire composition is grounded in the narration of a landscape designed to show 24 time gardens giving the public immediate topographical orientation within the matrix of global­ised conflict.

Tell me more

View Case Studies

Up to 170 years of protection

Find out how long galvanizing will last in your area and view a list of approved galvanizers near you...

Hot dip galvanizing corrosion map

This map provides data for the atmospheric corrosion rate of hot dip galvanizing. Search for a location and hover over the 10 km grid to obtain the corrosion rate. The map legend can be used to find the average life of an 85 µm coating within the area.

Corrosion rate key
Average Corrosion Rate(µm/year) 0.5 1 1.5 2 2.5
Average Life of 85µm galvanized coating(years) 170 85 57 43 34

Average background corrosion rates for zinc. Each grid square is 10km².