It is astonishing to think that a coating, just thicker than a sheet of A4 paper, can protect a steel structure for the better part of one hundred years.

What is the thickness of a galvanized coating?

When it comes to the specification of hot dip galvanizing, most contractors know that to be standards compliant, 7mm steel requires an average coating thickness of ‘85 microns’. It is a simple industry standard that is easy to retain and is applicable to many construction needs.

But how does that microscopic coating translate into performance? And what does ‘85 microns’, actually look like? 

Under the international system of units (SI) the micron is represented by the Greek symbol μm, which signifies one thousandth of a millimetre. To put that in perspective, it is often cited that the human eye can perceive objects no smaller than 40 microns and that the average human hair is a mere 50 microns in diameter. Cling film comes in at 10-12 microns thick and a typical bacterium is 1-10 microns long.

In fact, an 85 micron galvanized coating can last for nearly a century in many UK atmospheric settings (click to see corrosion rates in your area). Not bad for a coating which, in cross section, is barely visible to the naked eye.

Hot Dip Galvanizing Thickness and Steel Thickness

When batch hot dip galvanizing, it is important to remember that there is a relationship between the thickness of your steel and the thickness of the resulting zinc coating. These variables are represented in the table below.

Hot Dip Galvanizing Thickness Chart

In general, the thicker the steel, the thicker the zinc coating obtained and the longer the lifespan of your protection. What these numbers conceal is that hot dip galvanizing produces a coating which is bonded metallurgically to the steel.

In addition to steel thickness, the composition of the steel alloy itself is also relevant. Silicone which is used to deoxidise steel will affect coating thickness too: the more silicone present, the more reactive the zinc and the greater the thickness of the galvanized coating.

The corrosion rate of a galvanized coating is generally linear.

How this microscopic coating then weathers is predictable but complex and fluctuates with atmospheric conditions. In most dry inland situations this can be infinitesimally slow, less than 1 micron per year, and unlike other coatings, a galvanized coating deteriorates in a linear fashion. As long as the environment remains stable, case studies show that the coating throws up no unpleasant surprises and can be relied upon.

Moreover, in the UK and Ireland, as sulphur dioxide levels have fallen, corrosion protection has been extended. It does indeed pay to know your microns.

Posted by Galvanizers Association on 26th February 2020

Join the conversation

Make a comment
Cancel

Browse by category

Dr Des GAGAs Learn it! Sustainability

Popular articles

RIBAJ Design Competition: Wanderer's Wonder

Posted on 9th September 2021

Wanderer’s Wonder is a new competition brought to you by RIBA Journal and Galvanizers Association th...

Reducing Whole Life Carbon Footprint by Avoiding Maintenance

Posted on 16th July 2021

According to the UK Green Building Council “depending on bui...

Durable Materials and Sustainable Growth

Posted on 2nd July 2021

According to Gov.UK, the UK construction sector is undergoing one of the biggest periods of expansio...