Newport Galvanizers Limited

Newport Galvanizers Limited

Address:
Llanwern Works
Newport
Gwent
NP19 4QX

Telephone: 01633 277400
Fax: 01633 277997
Email: newport@wedge-galv.co.uk
Website: http://www.wedge-galv.co.uk/

Bath size:
6.8m x 1.1m x 3.5m

Double dip:
Sizes on application

Max lift: 10 tonnes

Main classes of work:
Structural
Tubular
General

Additional features and services:
Awarded “Investor in People”
Registered to BS EN ISO 9002
Centrifuge for spin galvanizing
Grit blasting
Painting after galvanizing