Galvanizers in Scotland

Forfar Galvanisers Ltd

Address:
Carseview Road
Forfar
Angus
DD8 3BT

Telephone: 01307 460 222
Fax: 01307 460 444
Email: enquiries@forfar-galvanisers.co.uk
Website: http://www.forfargalvanisers.co.uk/

Bath size:
5.5 m x 1.5 m x 2.8 m

Double dip:
Not available

Max lift: 1.4 tonnes

Main classes of work:
Structural
Pallets
Tubular
Gates
Fencing
Agricultural
General

Additional features and services:
Transport available
Shotblasting
Pickling

Highland Colour Coaters Ltd

Highland Colour Coaters Ltd

Address:
2 Tower Road
Cumbernauld
G67 2JH

Telephone: 01236 731444
Fax: 01236 731555
Email: enquiries@higalv.co.uk
Website: http://www.higalv.co.uk/

Bath size:
7.0m x 1.2m x 3.0m

Double dip:
Sizes on application

Max lift: 4 tonnes (powder coating 750kg per item)

Main classes of work:
Agricultural
Tubular
Fencing
General

Additional features and services:
Powder Coating
Centrifuge for spin-galvanizing
Electroplating
Shot blasting
Transport Service
Registered to BS EN ISO 9001

Highland Galvanizers

Highland Galvanizers

Address:
3 Pinefield Parade
Elgin
Moray
IV30 6FG

Telephone: 01343 548855
Fax: 01343 545551
Email: enquiries@higalv.co.uk
Website: http://www.higalv.co.uk/

Bath size:
10.4 m x 1.05 m x 2.5 m

Double dip:
To 15m long
Call for specifics

Max lift: 4 tonnes

Main classes of work:
Agricultural
Offshore/Marine
Structural
Tubular
Fencing
Centrifuged
General

Additional features and services:
Registered to BS EN ISO 9001
Centrifuge for spin galvanizing
Electroplating
Fabrication
Grit blasting
Painting after galvanizing
Thread brushing
Transport service

Scottish Galvanizers Limited

Scottish Galvanizers Limited

Address:
Maclellan Street
Glasgow
G41 1RR

Telephone: 0141 427 3041
Email: scottish@wggltd.co.uk
Website: http://www.wedge-galv.co.uk/

Bath size:
14.2m x 1m x 2.9m

Double dip:
Double dip up to 21m length

Max lift: 10 tonnes

Main classes of work:
Structural
Tanks
Castings
Tubular
General
Centrifuged

Additional features and services:
Registered to EN ISO 9001:2015
Centrifuge for spin galvanizing
Grit blasting
Transport service