Bridge infrastructure, Gabon

galvanized-bridge-map-gabonA journey through Gabon will take in a vast country criss-crossed by rivers, forests and an abundance of wildlife. What quickly becomes apparent is the lack of connection across key routes through the country. A new government backed investment programme is trying to address these issues with the help of Acciona, an infrastructure company based in Spain.

Acciona were set the task of working on two routes on the western and eastern fringes of the country; Lambarene, where 42 bridges needed to be replaced and Kelle – Akieni which involved 38 bridges.

Acciona’s engineering team decided to tackle the numerous problems they faced by adapting a modular concept for the bridges. This would enable the design to be adapted to local on-site conditions of varying spans, loading and erection methods. A substantive remit of the client was that of the requirement to have the bridges designed with a maintenance free service life.

Steel become the material of choice for its strength to weight properties, and hot dip galvanizing as the protective coating that would be necessary to provide the required protection in what would be a tropical, humid environment. During the manufacturing phase, fabrication was carried out to tight tolerances with the added focus of enabling interchangeability of some sections. Given the importance of corrosion protection, steel containing optimum levels of silicon and phosphorus was specified to obtain a thicker galvanized coating.

The project has not only improved the daily lives of villagers but brought whole communities together, part of which involved the training of local labourers to erect and perform load tests on the the bridges.

Image: Acciona Infrastructures, Acciona Engineering, S.A

Posted on January 17, 2017 by Galvanizers Association

Read next…

Almere Windhinders, Amsterdam

A series of new canopy structures weave their way through the city centre in Almere, a new town just outside Amsterdam. The canopy, along with a flower stall form a series of interventions critical to the commercial success of the…

Read more

Catwalk in Santa Pola, Spain

Can a balance be struck between preservation of an ecologically important area, while catering for its popularity as a tourist destination? This was the conundrum faced by authorities in Santa Pola. Located south of Alicante on the Mediterranean coast, Santa…

Read more

Crossrail Place, London

In 2008, Foster + Partners were commissioned to design a mixed-use scheme encompassing the over-ground elements of a new station for the Crossrail project at Canary Wharf. Central to the scheme, was a new enclosure unifying the station and other elements…

Read more

Galvanized reinforcement for concrete structures

Reinforced concrete is a widely used material within construction with an attractive range of properties and characteristics. It can be used in a variety of exposure conditions, however attention needs to be given to the potential for steel reinforcement within…

Read more