Image: Institut Feuerverzinken

Reinforcing the past

Reinforcement of A67/A3, Frankfurt

It is a well known fact that hot dip galvanized steel can be used in the construction of new infrastructure. It should not be forgotten that it can also play an important role in retrofitting structures. This can prolong the life of existing structures, increase capacity and with the work being carried out while the structure is still in use, avoid delays and additional expense.

A good infrastructure strategy will include the building of new structures with the sustainable use of resources. In addition to this, retrofitting should be considered to be an important element within this strategy. Retrofitting can often take place without any significant interference in traffic and thus avoid congestion that increases costs and have negative environmental impacts.

Hot dip galvanized steel has emerged as the preferred material for the strengthening of bridge structures. Its strengths include maximum prefabrication, ease of assembly, relatively low component weight, robustness and maintenance-free durability.

A example is the reinforcement of the A6/A3 feeder bridge at the Mönchhof triangle near Frankfurt. The reinforced concrete bridge transfers the feeder from the A6 to the A3. Galvanized CHS sections help to brace the concrete piers and a galvanized steel frame at the bridge abutment helps to transfer superstructure loads onto a new strip foundation.

Subscribe to Hot Dip Galvanizing Magazine

Image: Institut Feuerverzinken

Posted on July 28, 2020 by Galvanizers Association

Read next…

Adidas Campus World of Sports

The Adidas Campus World of Sports building in Herzogenaurach is the corporate headquarters of the brand. In 2019 it was extended to include a new foyer designed by Behnisch Architects. The striking, flat cuboid with its diamond-shaped facade and its…

Read more

Batelease Farm, Devon

The client had initially approached the architects in 2013 to design an extension to their grade ll listed farmhouse, on a footprint, that the house had originally stood on before being flattened by a stray bomb during World War II.…

Read more

Heini-Klopfer ski jump, Oberstdorf

The is the third largest in the world. The ski jump, originally designed by the architect and ski jumper Heini Klopfer in 1950, was refitted in 1973 and 1986. A more thorough renovation of the ski jump was carried out…

Read more

Private house in Belgium

If the energy of solar radiation can penetrate a system almost unhindered, but the outflow of heat is restricted, this is called the glasshouse or greenhouse effect. While this effect is increasingly becoming a problem for the earth, a family…

Read more