Galvanizing to Standard EN ISO 1461 [HDG Datasheet 4b]
The European and International standard covering post-fabrication hot dip galvanizing of steelwork EN ISO 1461 : 2022 Hot Dip Galvanized Coatings on Fabricated Iron and Steel Articles – Specifications and Test Methods, covers the galvanizing of steel fabrications, sections and castings in a bath of molten zinc containing a minimum of 98% zinc.
Â
The standard excludes products processed by an automated process such as sheet, wire and tubes.
The datasheet offers information on the following:Â
- The key points covered within the standard
- Inspection Procedure
- Required number of reference areas for testing
- Surface Finish
- Coating Thickness
- Repair
- Coating Adhesion
- Acceptance Criteria
- Certification
Request a free pdf of this datasheet.