HDG Datasheet 4a: Specifying Hot Dip Galvanized Steel | Galvanizers Association

HDG Datasheet 4a: Specifying Hot Dip Galvanized Steel

For the vast majority of applications, hot dip galvanizing can be simply specified using the following reference: Hot dip galvanized to BS EN ISO 1461 : 2009 by a member of Galvanizers Association.

HDG Datasheet 4a - Specifying Hot Dip Galvanized Steel

The standard contains coating thickness requirements which will typically be sufficient to achieve an acceptably long coating life.

The datasheet offers information on the following:

  • Minimum coating thicknesses achieved by hot dip galvanizing to BS EN ISO 1461 (not centrifuged)
  • Nominal coating thicknesses on samples that are grit blasted prior to hot dip galvanizing
  • Thicker coatings by surface roughening
  • Use of a reactive steel

Want to have a pdf version of this datasheet? Click the button below.